Тяговое усилие 12 lbs — 900 lbs
Ориентация намагниченности Axial
Grade Max. Operating Temperatures
N35-N52 80°C (176°F)
Remanence(Br) 11,300 Gauss — 14,800 Gauss
Coercive Force(Hcb) 10,000 Oersted — 11,600 Oersted
Intrinsic Coercive Force(Hcb) 11,000 Oersted — 12,000 Oersted
Magnetic Energy Product (BH) 33M GOe — 53M GOe
11,300 Gauss — 14,800 Gauss
10,000 Oersted — 11,600 Oersted
11,000 Oersted — 12,000 Oersted
Grade Max. Operating Temperatures
N35-N52 80°C (176°F)
Remanence(Br) 11,300 Gauss — 14,800 Gauss
Coercive Force(Hcb) 10,000 Oersted — 11,600 Oersted
Intrinsic Coercive Force(Hcb) 11,000 Oersted — 12,000 Oersted
Magnetic Energy Product (BH) 33M GOe — 53M GOe
Обработка поверхности Ni-Cu-Ni, Nickel, Zn